Concrete Technology — Worked Examples
These examples follow the concrete quality chain from fresh testing and mixture proportioning through hardened strength and nonconformance investigation. Acceptance decisions always defer to the governing project specification and code.
Example 1 — Water-cementitious materials ratio
A concrete mixture contains Portland cement, fly ash, and effective mixing water. Determine .
Step-by-Step Solution
0 of 2 Steps CompletedExample 2 — Interpret an invalid slump observation
During a slump test, the concrete mass shears markedly to one side rather than subsiding uniformly. The technician records the largest vertical difference as 160 mm. Decide how the observation should be handled.
Step-by-Step Solution
0 of 3 Steps CompletedExample 3 — Absolute-volume fine-aggregate calculation
For of trial concrete: cement = 360 kg with relative density 3.15; water = 180 kg; SSD coarse aggregate = 1050 kg with bulk SSD relative density 2.65; air = 1.5%; SSD fine-aggregate relative density = 2.60. Determine SSD fine-aggregate mass.
Step-by-Step Solution
0 of 3 Steps CompletedExample 4 — Aggregate moisture correction
The SSD trial proportions require 1050 kg coarse aggregate and 766 kg fine aggregate. Coarse aggregate absorption is 0.5% and total moisture is 2.0%; fine aggregate absorption is 1.2% and total moisture is 6.0%. All percentages are on an OD basis. Design mixing water is 180 kg. Determine wet aggregate masses and added water.
Step-by-Step Solution
0 of 3 Steps CompletedExample 5 — Concrete density and measured yield
A trial batch uses a total batched mass of and fills a calibrated measure with of concrete. The batch was intended to produce exactly . Estimate fresh-concrete density and actual yield.
Step-by-Step Solution
0 of 3 Steps CompletedExample 6 — Cylinder compressive strength
A diameter concrete cylinder fails at a maximum load of during a valid cylindrical compression test. Determine measured compressive strength.
Step-by-Step Solution
0 of 3 Steps CompletedExample 7 — Investigate an unexpectedly low strength test
A valid project strength report is unexpectedly below the acceptance trend. Determine the investigation sequence before changing the mixture or condemning the structure.
Step-by-Step Solution
0 of 4 Steps CompletedExample 8 — Placement and segregation control in a congested wall
Concrete is discharged from high above its final location, repeatedly striking reinforcement, while workers add unauthorized water to make it flow. Identify the material-quality risks and controls.